Effect of surface cleaning prior to chemical strengthening process of glass

Atilgan S, Ozben N, Sokmen I, Wondraczek L, Akman S (2020)


Publication Type: Journal article

Publication year: 2020

Journal

Book Volume: 11

Pages Range: 720-729

Journal Issue: 4

DOI: 10.1111/ijag.15479

Abstract

This work focuses on the effect of surface cleaning treatments of soda-lime-silicate float glasses before chemical strengthening where a compressive stress layer is introduced via ion exchange. As-received and cleaned glass surfaces were subjected to two different treatments using demineralized water and acidic solutions were subjected to ion exchange in a molten KNO3 bath for 8 hours at 450°C. Precleaning treatment leads to a relative enhancement of the potassium surface concentration following chemical strengthening as compared to the uncleaned samples, also reflecting in altered surface stress profiles and case depth. These observations provide guidance for optimal pretreatment conditions of glass for chemical strengthening. Appropriate cleaning treatments can result in higher achievable fracture loads of subsequently chemically tempered glasses in ring-on-ring biaxial bending tests.

Authors with CRIS profile

Involved external institutions

How to cite

APA:

Atilgan, S., Ozben, N., Sokmen, I., Wondraczek, L., & Akman, S. (2020). Effect of surface cleaning prior to chemical strengthening process of glass. International Journal of Applied Glass Science, 11(4), 720-729. https://doi.org/10.1111/ijag.15479

MLA:

Atilgan, Semin, et al. "Effect of surface cleaning prior to chemical strengthening process of glass." International Journal of Applied Glass Science 11.4 (2020): 720-729.

BibTeX: Download