Adhesive Failure of Lava Ultimate and Lithium Disilicate Crowns Bonded to Zirconia Abutments: A Prospective Within-Patient Comparison

Beitrag in einer Fachzeitschrift


Details zur Publikation

Autorinnen und Autoren: Schepke U, Lohbauer U, Meijer HJ, Cune MS
Zeitschrift: International Journal of Prosthodontics
Jahr der Veröffentlichung: 2018
Band: 31
Heftnummer: 3
Seitenbereich: 208-210
ISSN: 0893-2174


Abstract

PURPOSE: To demonstrate the influence of restorative material on the success of clinical bonding to zirconia.
MATERIALS AND METHODS: A total of 50 participants with a single implant received screw-retained restorations; ie, Lava Ultimate (LU) crowns extraorally bonded to zirconia abutments. After 1 year, lithium disilicate (LDS) was used as an alternative restorative material. These restorations were also followed for 1 year.
RESULTS: Forty LU restorations (80%) debonded within 1 year of clinical service, whereas no bonding failures occurred with LDS restorations.
CONCLUSION: The choice of restorative material for single crowns luted to zirconia implant abutments strongly influences the incidence of bonding failures.


FAU-Autorinnen und Autoren / FAU-Herausgeberinnen und Herausgeber

Lohbauer, Ulrich Prof. Dr.
Medizinische Fakultät


Zusätzliche Organisationseinheit(en)
Zahnklinik 1 - Zahnerhaltung und Parodontologie


Einrichtungen weiterer Autorinnen und Autoren

University of Groningen / Rijksuniversiteit Groningen


Zitierweisen

APA:
Schepke, U., Lohbauer, U., Meijer, H.J., & Cune, M.S. (2018). Adhesive Failure of Lava Ultimate and Lithium Disilicate Crowns Bonded to Zirconia Abutments: A Prospective Within-Patient Comparison. International Journal of Prosthodontics, 31(3), 208-210.

MLA:
Schepke, Ulf, et al. "Adhesive Failure of Lava Ultimate and Lithium Disilicate Crowns Bonded to Zirconia Abutments: A Prospective Within-Patient Comparison." International Journal of Prosthodontics 31.3 (2018): 208-210.

BibTeX: 

Zuletzt aktualisiert 2018-23-10 um 10:08